环氧地坪漆對水泥基面有哪些要求

文章时间:2019-02-24 12:26:33   浏览次数:1297

环氧地坪漆對水泥基面有哪些要求1、水泥基面牢固、結實、不起殼。杜絕砂漿起殼現象。最好混凝土層與砂漿找平層一起澆註:如果先搗混凝土層,則要求砂漿層的厚度不低於4cm,叉車道則要求更厚一些。
What are the requirements of epoxy floor paint for cement base surface? 1. Cement base surface is firm, firm and can not shell. E环氧地坪liminate the phenomenon of mortar shelling. It is better to pour the concrete layer together with the mortar leveling layer: if the concrete layer is tampered first, the thickness of the mortar layer should be no less than 4cm, and the forklift lane should be thicker.
2、要求表面不起砂,硬度好。沒有水泥粉化現象。要求A、優質水泥。B、新倒水泥砂漿層要充分保養。
2. Require no sand on the surface and good hardness. There is no cement pulverization. Requirements A, high quality cement. B. The newly pou透水地坪red cement mortar layer should be fully maintained.
3、水泥基面平坦、無凸凹不平、蜂窩麻面、水泥疙瘩。
3. The cement base surface is flat, without bumps, honeycomb linen surface and cement keloid.
4、要求地面平整性不大於塗裝要求厚度(用3米直尺平靠);
4. Require that the surface flatness should not be greater than the required coating thickness (with 3 meters ruler flat);
5、表面幹燥,含水量小於6,保持地面幹燥無油污.切記水泥地面保養期過後進場施工前5天,不能用水沖洗或拖把拖地。
5. Surface is dry, water content is less than 6, keep the ground dry and free from oil pollution. Keep in mind that after the maintenance period of the cement ground, you can not wash or mop the ground with water five days before entering the construction site.
6、环氧地坪表面的PH值應在6.0-8.0。
6. The PH value of the floor surface should be 6.0-8.0.
7、地面無油污、其他油漆、乳膠漆、泡泡糖等殘渣;坡度應符合設計要求,允許偏差值為坡度的2%,並且不大於30mm。
7. There is no oil stain, other paint, latex paint, bubble sugar and other residues on the ground; the slope should meet the design requirements, and the allowable deviation value is 2% of the slope, and not more than 30 mm.