導致鋼化环氧地坪出現色斑的因素

文章时间:2018-11-10 01:37:13   浏览次数:1213

鋼化环氧地坪在施工過程中以及施工完成後期會出現色斑,導致項目整體出現色素不均問題,影響效果和使用。下面為大傢分析介紹环氧地坪出現色斑的因素和處理辦法有哪些,來具體瞭解。鋼化环彩色沥清地坪氧地坪出現色斑的因素和處理辦法整理
Steel epoxy floor will be stained in the construction process and in the later stage of construction, resulting in uneven pigmentation of the project as a whole, affecting the effect and use. Below for you to analyze and introduce the epoxy flooring stain factors and treatment methods, to understand in detail. Factors and treatment methods of pigmentation on tempered epoxy floor
环氧地坪漆施工顏料不穩定會產生變色或者是退色。復色漆因各種顏料相對密度不同,儲存過程中發生沉淀和懸浮的狀態不同,在塗裝時又未充分攪拌均勻,造成塗刷時色差不同。如藍色漆或草綠漆,由於包裝桶內空氣不足,在儲存中發生還原作用導致退色。酞菁藍與酪黃配制的綠色漆,由於是有機顏料和無機顏料相結合,相對密度不同,鉻黃很容易下沉凝聚,酞菁藍上浮而使黃綠色變藍綠色。
The construction of epoxy floor paint will cause color change or fade. Due to the different relative density of various pigments, precipitation and suspension occur during storage, and the paint is not fully stirred uniformly, resulting in different color difference during painting. For example透水地坪, blue paint or grass green paint, due to insufficient air in the packaging barrel, reductive effect occurs during storage leading to discoloration. The green paint prepared by phthalocyanine blue and casein yellow is a combination of organic pigments and inorganic pigments. Because of the different relative density, chrome yellow is easy to sink and condense, and phthalocyanine blue floats up and turns yellow-green to blue-green.
环氧地坪漆施工中,金屬色漆的塗裝後,金屬粒子及著色顏料粒子在塗膜中會呈有序排列。在塗覆清漆層以後,清漆中的溶劑會使金屬色漆溶解,金屬粒子及著色顏料粒子根據流淌現象會發生遊離,並且進入到清漆塗膜中。
In the construction of epoxy floor paint, the metal particles and coloring pigments will be arranged in an orderly manner after the metal-colored paint is coated. After varnish coating, the solvent in varnish will dissolve the metallic paint, metal particles and pigments particles will dissociate according to the flow phenomenon, and enter the varnish film.