水磨石环氧地坪因為花色可隨意拼接、施工方便、造價低廉等特性廣受歡迎,從最開始的工業領域到如今的商業領域,水磨石环氧地坪的熱度一直不見減少,在超市、商場、飯店以及傢裝都場所都能看到它的身影。光亮度一直是水磨石地面的一個很亮眼的特點,可以說,大部分還是很喜歡水磨石地坪的花色和光亮度,所以才是選擇做水磨石地坪。不過有的時候水磨石地面在施工完成後會出現表面黯淡,光澤度明顯達不到標準的的問題。至於為什麼會出現這樣的問題,絕大多數人都是不明所以。下面小編就簡單講講水磨石地面光亮度差的原因以及解決方法。
Terrazzo floors are popular because of the characteristics of freely splicing, convenient construction and low cost. From the beginning of the industrial field to today's commercial field, the heat of terrazzo floors has not been reduced. It can be seen in supermarkets, shoppi环氧地坪ng malls, restaurants and home furnishings. Brightness has always been a very bright feature of terrazzo floors. It can be said that most of them still like the color and brightness of terrazzo floors, so they choose to be terrazzo floors. However, sometimes the terrazzo surface will be dim after the completion of construction, and the gloss can not reach the standard obviously. As for why such a problem occurs, most people are not aware of it. The following is a brief introduction to the reasons for the poor brightness of terrazzo floor and the solution.
一、水磨石地面光亮度差的原因
1. Reasons for poor brightness of terrazzo floor
1、磨光時磨石規格不齊,使用不當
1. When grinding, the specifications of the grindstone are uneven.
水磨石地面在施工時,磨光次數一般不應少於3次。不過在施工中,用到的禁房事砂輪往往規格不齊,並且對第二遍和第三遍的磨石要求不夠重視,隻要求石子、分隔條清晰可見,卻忽略瞭對表面光亮度的施工要求。
In the construction of terrazzo floor, the frequency of polishing should not be less than 3 times. However, in construction, the specifications of forbidden grinding wheels used are often uneven, and the second and third times of grinding stone requirements are not enough attention, as long as the stone, separator bars are clearly visible, but the construction requirements of surface brightness are ignored.
2、打蠟錢沒有塗抹草酸溶液
2, waxing money did not apply oxalic acid solution.
水磨石地面在打蠟前都是要塗抹草酸溶液的,並且如果不是塗抹溶液而是用粉狀草酸進行幹擦的話,會很難保證草酸在地面的均勻性。擦洗後,地面表面的潔凈程度不一致,沒擦幹凈的地方就會出現斑痕,直接影響打蠟的效果,造成水磨石地面光亮度低。
The terrazzo floor is coated with oxalic acid solution before waxing, and it is difficult to ensure the homogeneity of oxalic acid on the ground if it is not coated with oxalic acid solution but dried with powder oxalic acid. After scrubbing, the cleanliness of the ground surface is inconsistent, and there will be spots where it is not cleaned, which directly 彩色沥清地坪affects the effect of waxing, resulting in low brightness of terrazzo ground.
3、使用刷漿法來補漿
3. Use the brush method to reinforce the pulp.
刷漿法補漿的缺點在於無法完全消除洞眼,隻會在洞眼上下形成一層薄膜,在打磨後洞眼依然存在,這會導致水磨石地面光亮度低。
The disadvantage of grouting by brushing method is that it can not eliminate the holes completely, but only form a layer of film above and below the holes. After polishing, the holes still exist, which will lead to low brightness of terrazzo floor.
二、水磨石地坪光亮度差的解決方法
Two. Solution to the difference of terrazzo floor brightness.
水磨石光亮度差並不需要敲掉重新施工,隻需要使用混凝土密封固化劑就可以提升地面的光亮度。混凝土密封固化劑可以封堵住水磨石地面表面的孔隙,使之成為一個密實的整體,再使用專業的打磨機器多層次打磨後,可以讓地面呈現出大理石般的光澤。並且會隨著使用時間的增加,光澤度也會增加。
The difference in brightness of terrazzo does not need to be knocked out and re-constructed, but only the use of concrete sealant curing agent can improve the brightness of the ground. The concrete sealing solidifying agent can block the pore of terrazzo surface and make it a compact whole. After multi-level polishing with professional polishing machine, the terrazzo surface can show marble-like luster. And the gloss will also increase with the increase of use time.
除瞭能夠增亮水磨石地面,混凝土密封固化劑還能達到硬化、強固、抗磨耗、防塵、防水、抗化學侵蝕、抗鹽分、抗油污、安全环保的固封效果,還能增加地坪的使用壽命,最高可達30年。
In addition to brightening terrazzo floors, concrete sealants can also achieve hardening, strong, anti-wear, dust-proof, waterproof, chemical erosion resistance, salt resistance, oil pollution resistance, safety and environmental protection of the sealing effect, but also increase the service life of the floor, up to 30 years.