环氧地坪上有水珠是怎麼回事?

文章时间:2018-11-03 21:39:44   浏览次数:1126

在环氧地坪施工時,环氧地坪會因為人為原因出現一些問題,不知道大傢有沒有見過环氧地坪“出汗”,一般這種現象通常會發生在环氧地坪打磨完成之後,有時我們會發現地面呈現光亮或者是有水珠,其實這種現象就是环氧地坪“出汗”瞭,不過並不是每一種地坪都會出現這種現象,主要是一些油性地坪表面,其實地坪會“出汗”是有很多原因造成的,比如說基面處理不徹底,導致底層的油脂或者是水分滲透到地坪表面等等。
During the construction of epoxy flooring, there will be透水地坪 some problems due to man-made reasons. I don't know if you have ever seen "sweating" of epoxy flooring. Generally, this phenomenon usually occurs after the ground is polished. Sometimes we will find that the ground is bright or has water droplets. In fact, this phenomenon is the "emergence" of epoxy flooring. Sweat, but not every kind of floor will appear this phenomenon, mainly some oily surface, in fact, the floor will "sweat" is caused by many reasons, such as the base treatment is not thorough, resulting in oil or water infiltration into the surface of the floor and so on.
环氧地坪“出汗”有很多原因,基本上有三條的是主要原因:
There are many reasons for sweating of epoxy floor. There are basically three reasons:
1、地坪漆膜沒有完全幹透就進行打磨。
1, the floor paint film is not completely dry to polish.
2、選用瞭非溶劑型的增塑劑,例如蓖麻油、樟腦等。一般出現在硝基漆。
2. Non solvent plasticizers such as castor oil and camphor were selected. Generally occurs in nitrocellulose lacquer.
3、漆膜中更含有蠟、礦物油等油脂。
3, paint film contains wax, mineral oil and other oils.
針對這樣的問題我們給出的對策:
In response to such problems, we propose countermeasures:
1、打磨地坪必須等漆膜徹底幹透以後進行。
1.印花地坪 Grinding floor must be thoroughly dried after coating.
2、增塑劑最佳挑選溶劑型的。
2. Plasticizer is the best solvent type.
3、盡量少用富含這些油類的添加物,或是找其他替代。
3, try to use less oil rich additives, or find other alternatives.
所以啊,大傢在施工時一定不能放松警惕,每一步施工都應該認真對待。選材上也要註意,還有就是施工方法不能半懂。
So, we must not relax our vigilance during construction. Every step of construction should be taken seriously. We should also pay attention to material selection, and the construction method should not be half understood.