环氧地坪雖然在現在比較常見的一種环氧地坪類型,但是环氧地坪在施工過程中也會由於各種問題,無法達到預想的效果,而常見的狀況就是环氧地坪表面粗糙, 針對於這種情況應該怎樣處理呢,在處理之前要分析一下原因,再根據原因找出相應的解決辦法。 耐磨地坪漆出現表面粗糙的現象主要以下四點:
Although the epoxy wear-resistant floor is a common type of floor now, the epoxy wear-resistant floor can not achieve the desired effect due to various problems in the construction process, and the common situation is that the surface of the epoxy wear-resistant floor is rough. In view of this situation, how to deal with it? Before dealing with it, we need to analyze one. Next, find out the corresponding solutions based on the reasons. The surface roughness of wear-resistant floor paint is mainly the following four points:
1、因為施工环境不幹凈,有較多的灰塵,灰塵黏在塗膜上就會出現粗糙;
1, because the construction environment is not clean, there are more dust, dust will stick on the film will be rough.
2、調配好的耐磨地坪漆材料沒有經過過濾就直接使用瞭,使雜質混入裡面,當塗膜幹燥之後就會在环氧地坪上顯示出來;
2. The prepared abrasion-resistant floor paint material is directly used without filtering, so that impurities are mixed into it. When the film is dried, it will be displayed on the epoxy floor.
3、耐磨地坪漆已經開始固化,仍然繼續施工,因為耐磨环氧地坪漆都是雙組分的,加入固化劑之後就會產生化學反應,然後固化成膜,如果已經開始固化,仍會施工完成,那就會導致粗糙;
3. The wear-resistant floor paint has begun to solidify, but still continues to be constructed, because the wear-resistant floor paint is two-component, after adding curing agent, it will produce chemical reaction, and then solidify in印花地坪to film. If it has started solidification, it will still be completed, which will lead to roughness.
4、施工現場的溫度太高,使得稀釋劑揮發速度快,耐磨地坪漆還沒有流平就已經固化。
4. The construction site temperature is too high, which makes the diluent volatilize quickly, and the wear-resistant floor paint has solidified before leveling.
相應的解決辦法有,在施工耐磨地坪漆之前一定要將基面及現場清掃幹凈,將耐磨地坪漆材料用過濾網過濾之後再施工。施工前要根據施工時間計算材料的用量,再嚴格按照塗料配比進行調配。不能多配,使用的稀釋劑需要慢幹的高飛點的。處理好下層,從底層開始就要按施工要求做好,中層要杜絕粗糙現象,面層施工前一定要把中層清理幹凈,確認無灰塵後再施工,這樣就可以解決耐磨地坪漆該類的粗糙現象瞭。
Corresponding solutions are: before the construction of wear-resistant floor paint, it is necessary to clean the base surface and the site, and filter the wear-resistant floor paint material with a filter before construction. Before construction, the amount of material should be calculated according to the construction time, and then stric环氧地坪tly allocated according to the proportion of the paint. It can't match well. Thinners need slow dry high flying points. To deal with the lower layer well, we should do a good job according to the construction requirements from the bottom layer. The middle layer should eliminate the rough phenomenon. Before the surface layer construction, we must clean the middle layer, confirm that there is no dust before construction, so that we can solve this kind of rough phenomenon of wear-resistant floor paint.