环氧地坪廠傢教您如何處理地坪表面不平整

文章时间:2018-11-03 04:13:24   浏览次数:1129

現在我們的生活中隨處可見各種各樣的环氧地坪,比如地下車庫,生產車間,球場等等。但是在施工結束之後,有時候會發現环氧地坪表面不平整,有雜物,看起來不美觀。可能好多朋友不知道為什麼會引起這種現象,下面簡單給大傢分析一下導致环氧地坪表面不平整的原因。
Now we can see all kinds of floors everywhere in 彩色沥清地坪our life, such as underground garage, production workshop, stadium and so on. But after the construction, sometimes the surface of the epoxy floor is uneven, there are debris, and it looks ugly. Maybe many friends don't know why it causes this phenomenon. Here's a brief analysis of the reasons for the uneven surface of epoxy flooring.
1)施工中雜質混入;
1) impurity in construction.
2)地面不平整,起伏過大或施作环氧地坪規格太薄;
2) uneven surface, undulating or too thin floor.
3)材料塗佈時,已部分反應,粘度過大,甚至產生硬塊;
3) when the material is coated, it has been partially reacted, the viscosity is too large, and even the hard lump is formed.
4)施工中斷料,來不及銜接。
4) construction interruption is too late to connect.
其實這些狀況經常會出現,隻要我們找出原因,對癥下藥就行,主要有一下幾點解決方法:
In fact, these situations often occur. As long as we find out the reasons, we can prescribe the right medicine. There are several main solutions:
1)环境力求清潔,石英砂應選擇顆粒均勻者;
1) environment should be clean a印花地坪nd quartz sand should be evenly distributed.
2)地面處理平坦,並清潔幹凈,凹處須修補,附著物須鏟除,依實際情況選做適當規格地坪;
2) The ground treatment is flat and clean, the concave areas need to be repaired, the attachments need to be removed, and the floor with appropriate specifications should be selected according to the actual situation.
3)材料前後塗佈,須在可使用時間銜接完畢。以免超過使用時間,材料粘度過大而無法自然流平,或桶內殘存部份塗料產生少許硬塊,此時應更換新桶。