环氧地坪工程中塗施工有哪些步驟
环氧地坪漆中塗施工步驟1)、計量工按石英砂配比(7號砂:9號砂=8.5:1.5),膠砂比1:1.5~2.0的要求把稱量好的环氧中塗樹脂和石英砂放入攪拌容器中,並做好用量度記錄,攪拌工先攪拌。2)、計量工按配合比依次準確稱量好固化劑放入攪拌容器中,同時將用量做好記錄。3)、攪拌工繼續攪拌,至少攪拌3分鐘,以保證混合均勻。4)、操作工用鏝刀均勻鏝勻。5)、說明:中塗樹脂若摻其他材料後,比重會有所變化,由實驗室提供,以確定單位面積使用量。厚度應符合設計單位和業主的要求。6)、膠泥層在養護24小時以上(夏季),冬季更長。自然硬化後,局部修整、打磨、吸塵,施工後養護大於24小時。
Epoxy floor paint intermediate coating construction step 1, metrologists according to the proportion of quartz sand (No. 7:9 sand = 8.5:1.5), sand ratio 1:1.5 to 2.0 requirements of good weighing epoxy resin and quartz sand into the mixing container, and do a good印花地坪 dosage record, mixer mixing first. 2) Metrologists accurately weigh the curing agent in 彩色沥清地坪the mixing vessel according to the mixing ratio, and record the dosage. 3) agitator continue stirring, stirring for at least 3 minutes to ensure uniform mixing. 4), the operator evenly trowel with a trowel. 5) Description: If the resin is mixed with other materials, the specific gravity will change, provided by the laboratory to determine the amount of use per unit area. The thickness should meet the requirements of design units and owners. 6), the mortar layer is maintained for more than 24 hours (summer), and winter is longer. After natural hardening, local dressing, grinding and vacuuming are carried out after construction for more than 24 hours.