环氧地坪工程結束後為何會起泡?

文章时间:2018-10-12 07:41:06   浏览次数:1157

基層的潮濕是主要的,絕對幹燥的基層是沒有的。所以泡都產生在平面上,多在基層與环氧層之間;基層中的水分是很難避免的,這就是造成环氧層起泡重要因素。环氧地坪漆有潮氣不能固化;那麼水分從何處來的呢?宇澤环氧地坪告訴您在环氧地坪施工後為何會有水泡發生,主要有以下幾個方面的原因:
The humidity at the grassroots level is the main and the absolute dry base is not. So bubbles are produced in the plane, mostly between the base layer and the epoxy layer; the water in the base layer is difficult to avoid, which is an important factor causing the epoxy layer foaming. When the epoxy floor paint has moisture, it can not solidify; where does the moisture come from? Yuze Floor tells you why blisters occur after the construction of epoxy floors. The main reasons are as follows:
1.基層、如水泥砂漿找平層,最大含水率達12%左右,基層的最大含水量大於找平層。
1. The maximum moisture content of base course, such as cement mortar leveling layer, is about 12%, and the maximum moisture content of base course is higher than that of leveling layer.
2.环氧中的其它配料內的脫水不盡。
2. other ingredients in epoxy are彩色沥清地坪 not dehydrated.
3.环氧和基層施工時結合不好留下空隙和环氧本身的化學活性,沒有完全固化或者是遇到潮濕氣沒有完全固化的殘留物或氣體。
3. The combination of epoxy and base course construction is not good enough to leave voids and the chemical activity of epoxy itself, not completely cured or encounter moisture not complet印花地坪ely cured residue or gas.
4.基層的地下滲透的潮濕氣體。
4. grass-roots underground infiltration of moist gas.